Participant
Do not depend on the pre-set schedules of your kiln. Learn to program it yourself and do so every firing.
As I tell my students, learn to “think like the glass”. Try to fire the glass (go through the schedule) in your mind, then set thte kiln. It helps.
Pre-sets are very general and made to be overkill.