Yes, you soak it. Form it to the master which has had a release put over it – can be cling film. Let dry. Fire to at least tack fuse temps. Sand to appropriate smoothness. Re-coat with hardner if necessary, fire again if so. Coat with kiln wash. Use. Store carefully, it is fragile.