fiber paper.
Home › Forums › Glass Fusing › General Fusing Discussion › fiber shelf paper 1/8″ › fiber paper.
July 4, 2010 at 8:12 pm #11668
Participant
You do not need to pre-fire the fiber paper…..
It gets a little soft after firing. If you are really careful, you might get a second firing out of it.
You do not need kiln wash with it.
I have never noticed any fumes or odor from it firing.
Vernelle