Faster schedule for small kiln
Home › Forums › Glass Fusing › General Fusing Discussion › Better Jewelry Firing Schedule – Help? › Faster schedule for small kiln
September 20, 2018 at 7:29 pm #13761
Participant
I have a small test kiln, shelf size 7×7”. My schedule takes only 90 minutes but does not bubble squeeze because my jewelry pieces are 2” and smaller.
1500 per hour
15 minute hold
done
Jennifer Beaudoin Moffitt
Beaudoin Jewelry