evenheat rampmster II kiln
Home › Forums › Glass Fusing › General Fusing Discussion › evenheat rampmaster II kiln › evenheat rampmster II kiln
April 26, 2017 at 9:26 pm #13701
Participant
I have the 23-13 and use the schedules I got with my evenheat pro. I have found that the 23-13 fires hotter by about 30 degrees.I am working to adjust the evenheat pro schedules to work with the 23-13 but haven’t perfected yet. I haven’t had any devitravacation problems. I haven’t tried it but the manual for the 23-13 says you can use ther sides and turn the top off. I think it’s under “other”. Hope I was able to help.