Hi Folks
Still having problems with acrylic paints from Thompson. They say you can use as normal paints, can mix colors put on thin or buttery thick. Am finding that i am removing bottom layer everytime I try to put on heavy.
So here is my question. want to do fine animal paintings on glass. What would you suggest as best enamels to use. All will become jewelry, most are on black glass so colors need to be vibrant. Would be nice if could be done in one or 2 firings and need to be capped.
Any suggestions. Also don’t want to put lots of money into it until we find the right enamels
Thanks