When drilling holes (especially with a drill press), PLEASE make sure you are drilling on fired glass with smooth edges only, if you plan on using your hands to hold the glass. Otherwise, clamp the glass down with a vice.
This is the Voice (of 10 stitches worth) of Experience.
Dana
Fused Glass Designs
dba Jester’s Baubles