Paul; Thank you for your quick response, I’m sorry but after I posted, I cut the green section out and am going to try fusing a new green section into the piece. I will say that all the pieces were cleaned before firing and the kiln was not opened during firing. The marks looked as if I had dragged something across the piece and were blackish in color and while the rest of the piece had a nice shine the marks had a flat finish. Next time I’ll wait for a response before swinging into action. Thank you again