Dog-boning
Home › Forums › Glass Fusing › General Fusing Discussion › System 96 Firing Schedule › Dog-boning
April 26, 2013 at 3:08 am #12901
Participant
Are you using two layers of glass? What is your firing schedule?
While I have heard people say that System 96 has uneven thickness, I would think for the average glass fuser this is a non-issue. I use 96 exclusively, and if I have any issues with the glass, it is more likely coming from my “technique” that anything to do with the glass itself!
Dana W.
Jester’s Baubles Fused Glass Designs