The schedule is:

300>900 hold 15

500>1100

100>1250 hold 30

9999>1475 hold 10

9999>950 hold 45

100>800

200>700

400>100

I can’t recall this problem in my old kiln, or maybe it’s just that my eye is keener now. Any suggestions? Would be grateful to be pointed in the right direction..