Devit reminder
Home › Forums › Glass Fusing › General Fusing Discussion › devitrification › Devit reminder
April 7, 2014 at 10:05 am #13314
Participant
Dana,
Thanks so much for that reminder! I was just cruizing through the posts here, and even after fusing for many years now had a piece ready to refire after sandblasting off the devit…and sure enough it was about to go in without the Spray A …except for your good reminder.
Funny how things happen like that.
Happy Day!
Jolinda