devit and venting
Home › Forums › Glass Fusing › General Fusing Discussion › Making small cabochons with opalescents pickup kiln paper. › devit and venting
June 19, 2013 at 1:19 pm #12973
Participant
I have been using a lower temp(usually about 15 to 30 degrees F) with about a 2-10 minute more soak time and haven’t had any problems with devit. I have never vented(because I always forget). As small as your glass is, you should be able to accomplish this with a lower temp quite easily. Remember the color of your glass with affect your fusing as well.