devit
Home › Forums › Glass Fusing › General Fusing Discussion › what to do about devit on slumped dish › devit
July 6, 2012 at 3:28 pm #12576
Participant
I have a question about devitrification and I don’t even know if I have it. I am new here and very inexperienced. I am not sure if the proper way to ask another question on this topic is to post a reply or write the author.
my problem is that when I slump a clear glass tray in my mold the horizontal surfaces on the bottom are a bit frosty. I don’t know if this is because of the mold or it is devitrifying. I don’t mind it really, I just wondered if it is a fault that I should correct somehow. The top surface is fine. I am slumping to 1240 f., hold 30 minutes.
Thanks for any thougts,
Brenda