Paul, when you refer to ” (50 degrees an hour or so) starting at about 1050°F and creep up to about 1225°F” are you saying to ramp at full speed to 1050, then creeping up at 50 degrees an hour to 1225?  Would you be willing to share your entire slumping schedule for this?  I’ve actually had the glass break in the middle before it had a chance to melt.