Cracked Kiln Shelf
Home › Forums › Glass Fusing › General Fusing Discussion › Cracked Kiln Shelf › Cracked Kiln Shelf
November 1, 2011 at 2:11 am #12259
Participant
Same thing happened to me doing the kiln pressed glass project. I normally have the shelf on 1/2 inch posts to even the heating, and I should have put the shelf directly on the kiln floor.
But all is not lost! I just cut up the broken shelf with a tile saw (using the tile blade) into 1″ strips to use as dams, holders for screen melts, etc.