Corelite Firing Schedule
Home › Forums › Glass Fusing › General Fusing Discussion › Corlite Shelf for Skutt g-1414 kiln › Corelite Firing Schedule
August 24, 2014 at 7:10 pm #12731
Participant
I have also recently purchased a corelite shelf and was wondering about the ramping recommendations. I typically ramp up at 200 degrees per hour to 1000, but then ramp at 600 to process temp on any given fusing. Is the recommended 200 dph for the corelite shelf to the1000 degree crytical hold, or is this 200 dph limit for all temps, including process and anneal temps.
Lydia