COE104
Home › Forums › Glass Fusing › General Fusing Discussion › firing schedule for coe 104 sheet glass › COE104
August 14, 2013 at 2:22 am #13038
Participant
The higher the COE, the lower the full fuse temperature. 104 usually full-fuses at about 1425. You can adjust the firing schedules found on this site accordingly.From what I am seeing the annealing temp is about 965-970 deg f.
Dana W.