Klock Kit has a catalog with any kind of mechanism and hands you might want.
Order sonething and they will keep sending the catalog for years.
A diamond coring bit (they come in a vatiety of sizes), a ring of puddy filled with water, a drill press, and a lot of patience will driill a hole in the center of a clock face.
Watch the distance between drill press post and center of work.