Capping Glassline paint
Home › Forums › Glass Fusing › General Fusing Discussion › Enamels or Other Paints for Fusing?? › Capping Glassline paint
March 30, 2011 at 2:18 pm #10881
Participant
Hi, I cap with clear fine frit. I let the paint dry overnight then put a generous layer of frit down on top . I try to even it out so there are no holes or low spots. It fuses wonderfully flat with no air bubbles.