Inactive

Buy some dichro scrap, wrap in paper and beat it with a hammer. Seriously.

There is dichro frit on the market but it is expensive and the bits of glass actually have too much dichro on them imo – they don’t flow or fuse well.



Paul
FusedGlass.Org