Depends upon the type of bubble, but you can fire upside down (bubble migrates toward the “top”, which will be the bottom when you flip and fire again — that ends up being a lot of firings), or drill out the bubble, fill with frit and refire. Or, just fire flat, but it would have to be a fairly long hold.
Dana W.
Jester’s Baubles Fused Glass Designs