bottle paint
Home › Forums › Glass Fusing › General Fusing Discussion › Slumping a Painted Bottle › bottle paint
April 18, 2012 at 2:02 pm #12511
Participant
Hey Barb. I had a bad experience with a pink and blue bottle that was coated or painted to give it the color. The give away is when the bottle changes color where the cap srews on if it is a different color or clear. The color completely burned off in the kiln and left a nasty smell as well. Just not worth it. I have not seen a white one before but I probably would not try it.
Keith
High rivers and clear skies