Borax Spray Bottle
Home › Forums › Glass Fusing › General Fusing Discussion › bottle devitrification › Borax Spray Bottle
December 17, 2013 at 12:45 am #12485
Participant
I use a small plastic spray bottle I got in the cosmetic section at WalMart. Works just fine. The borax spray is just like water. It doesn’t get thick.
Barb