The bubbles are small and just under the surface, not burst.
The fusing schedule I use is
300 dph, 1000, hold 2 min; 300 dph, 1150, hold 15 min; 600 dph, 1250, hold 20 min; 600 dph, 1480, hold 20 min; AFAP. 100, hold 60 min; 90 dph, 960, hold 60 min; 120 dph, 750, hold 10 min; 300 dph, 100, hold 0 min.
I let the kiln cool down for about 12 hours after the firing just to be extra cautious.
I am a novice and am not really sure about the bubble squeeze.