Bisqueware

#13080
wordana
Participant

In some instances the bisqueware may not be as flat on the bottom, but then some “high quality” molds you get aren’t either. You can use bisque, just make sure to drill a couple of holes in the bottom to let air escape. Drill from the top down, because it will chip out a little when you go through the other side.

Dana W.

Jester’s Baubles Fused Glass Designs

http://www.jestersbaubles.com