Bending temp
Home › Forums › Glass Fusing › General Fusing Discussion › Blister and air bubbles in fusing result › Bending temp
February 20, 2011 at 7:54 pm #11194
Participant
If I were using the firing times below, during which phase is “bending temp” to open kiln and use stainless steel spoon to try to flatten air bubble…. below is the firing times that I will use.
FULL Fuse
1 300 1150 30
2 400 475 10
3 9999* 950 60
4 150 800 10
Or do you have a suggested firing schedule?
3 9999* 950 60
4 150 800 10