At that size rigidized fiber blanket probably would not support the weight without splitting.
I would seek out a potter to make what you want. You can achieve the multi step firing with a single mold by filling it with various amounts of dry plaster for the initial slumps.
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com