Are you …
Home › Forums › Glass Fusing › General Fusing Discussion › Primo Primer Kiln Wash › Are you …
February 15, 2011 at 12:10 am #11903
Participant
coating them 4 to five time and letting it dry between and also doing the brush strokes in different strokes with each layer? I usally get about 3 full fuse with mine.