Are you tapping the back of

Home Forums Glass Fusing General Fusing Discussion cutting glass Are you tapping the back of

#12966
Stephen Richard
Participant

Are you tapping the back of the glass along the score line?  This will give you angles.  You could go to the Bullseye site, education section where they have a note on “improving your glass cutting skills” which I have always found useful.

Stephen Richard

blogs at: http://www.verrier-glass.blogspot.com/ and  http://www.glasstips.blogspot.com/