Any shelf or fiber paper
Home › Forums › Glass Fusing › General Fusing Discussion › Optimizing Slumped Surface Appearance › Any shelf or fiber paper
October 13, 2015 at 3:05 am #13551
Inactive
Any shelf or fiber paper will contribute to hazing problems.
The best way to keep the bottom surface shiny is to stop the slump just before the glass hits the mold. This takes careful observation and some practice – but the payoff can be huge.
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com