adhesives for holding glass temporarily
Home › Forums › Glass Fusing › General Fusing Discussion › need help with glasstac › adhesives for holding glass temporarily
July 21, 2009 at 6:04 am #11372
Participant
I use diluted PVA (school glue/ Elmer’s etc). I place a drop at the edge of the glass. This is dry in 5-10 mins. The dilution is about 1 part glue to 20 parts water. No problems so far, but I use it as little as possible, prefering to build in the kiln rather than add a possible contaminant.
Stephen Richard