Achieving bubbles…
Home › Forums › Glass Fusing › General Fusing Discussion › How do I get those bubbles? › Achieving bubbles…
May 10, 2009 at 9:46 pm #11298
Participant
Hi Roxane, I will try sifting–that’s a new idea. And I’ll get some borax too. These have worked for you? My small kiln seems to require a slightly higher temp so I fuse at 1505. I also add in an anneal before that at 1250 for 20 mins. I got better results w/ all my fusings afterI built that extra anneal in. Thanks for your help.