I use liquid hairspray (the cheapest kind) either sprayed over the entire surface, or applied through a dropper where required. This takes about 5 mins to set. Glastac or glastac gel is made for the job, takes much longer to set so you can move things around for much longer than with hairspray before you settle on the final configuration, but I don’t find quite as reliable. I try to avoid Elmer’s glue (PVA) as it can leave marks when fired if too much is used.