Reply To: Draped tealight holder
Home › Forums › Glass Fusing › General Fusing Discussion › Draped tealight holder › Reply To: Draped tealight holder
December 11, 2019 at 4:33 pm #15059
Participant
I have used little Stainless Steel 4oz sauce cups to drape tealight holders over. They work great and cost about $2 each. Find in any Kitchen store. Put on a cookie sheet, heat in your oven to about 500 degrees and apply kiln wash. This takes awhile as you need to keep reheating and applying to get a nice coat of kiln wash to stick, but I have great success. Made 24 drape molds this way and a batch of votive holders. You can get about 2-3 drape firings out of 1 coating of kiln wash. Good luck