June 14, 2019 at 10:54 pm #14894
Participant
I have a problem, with clear dots, fused but they all have thin fire on the bottom. I’ve made many dots or frit balls, but never had this happen before! I was fusing 96coe, lowered the kiln heat & time. I’ve soaked them in white vinegar, Klear & water with Dawn dish soap added. Still white attached! Anyone with an idea how to remove Thin Fire Paper?