Better Jewelry Firing Schedule - Help?

Hi everyone,

I'm new to the forum, so I apologize in advance if you've heard this quesiton before.  I'm looking for a faster fusing schedule for small jewelry pieces.  All the ones I've tried take hours.  I took a class years ago, before I got my kiln and we fused small pieces in a matter of an hour or two.  Of course now that I have one, I can't finds a schedule that fuses very quickly.   I've found some fast fusing schedules, but I'm a little confused.  I'm using Spectrum 96 and a Paragon Firefly kiln.  Currently, my small cabochons are taking about 4 hours to fuse.   Help?

Thanks in advance!  Gina B

Faster schedule for small kiln

I have a small test kiln, shelf size 7x7”. My schedule takes only 90 minutes but does not bubble squeeze because my jewelry pieces are 2” and smaller.

 

1500 per hour

15 minute hold

done

 

Jennifer Beaudoin Moffitt

Beaudoin Jewelry

Thank you so much!

Thanks so much. This is so appreciated!  My pieces are 2” or less. I’m going to give this a try. Thanks again!

Thank you!

Does this mean AFAP to 1500 then hold for 15 minutes?  Still learning the process  

Thank you!

Does this mean AFAP to 1500 then hold for 15 minutes?  Still learning the process  

I apologize for being

I apologize for being cryptic.

Seg 1 [there is only one segment]

1500 Rate/hour

Hold 15 min

Let cool for 8-12 hours.

Takes about 90 minutes, then cooling time.

Jennifer Beaudoin Moffitt

Beaudoin Jewelry