Error on firing schedule page?

I primarily work with float glass, but I have a small job making something using some Bullseye, so I found your firing schedule pages.  On the schedule for firing to full fuse, 6mm glass, everything makes sense until the final annealing ramp down "time for segment", which states that going from 700 to 100 at 400/hr would take 4:48.  Due to my age, I checked to see if I might be going senile, and just "don't understand", but I think the computer keyboard malfunctioned at some point.Smile

Error on firing schedule page?

Hello.

Am quite new around here but just looked over the firing schedule in question and the spreadsheet that generated the 4:48 time.  The spreadsheet in the download has some logic built in that accounts for your particular kiln's maximum ramp capability (both going up and down in temperature).  If the specified ramp is greater than the max ramp then the value from the "max ramp" table is substituted in the time calculation.  Note ther orange color of the spreadsheet cells and the accompaning notes.  Pretty cool.

Bob

Comment viewing options

Select your preferred way to display the comments and click "Save settings" to activate your changes.