Does glass fade?

Hi Fellow Fusers

Does anybody know whether or not the sun fades glass?  I have all of my glass, supplies, tools, kiln, etc in my Florida room. It gets very sunny in there and the large windows are not protected. Thanks. Jackie

Not that I have ever heard

Not that I have ever heard of.  Stained glass windows that are hundreds of years old are just as vibrant (when clean) as when they were  made.

----------------------
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com

 

Thanks Paul.

Thanks Paul.