Hi-temp decals interest me for use in pendant making, but I don't like the look of one placed on the surface of a piece. Is it possible to place one on top of the bottom layer of a two layer piece (in other words between the two layers) and then do a full fuse? If so, what is a good source for hi-temp decals?

i haven't tried this yet

I haven't tried this yet, but I was under the impression that you could put a decal on your glass and put transparent glass on top of it.  I'm sure it says on the package though.

Thanks for the reply - I

Thanks for the reply - I guess I'll just have to experiment, eh?

This thread talks about

This thread talks about custom high temp decals, but also touches on capped or uncapped fusing.

http://www.warmglass.com/phpBB/viewtopic.php?f=2&t=40971&p=349900&hilit=decals#p349900