Fold-Over Pendant Tutorial

Ask any group of jewelry fusers what glue is best for attaching metal bails to glass and you are certain to hear a variety of opinions - often contradictory.

An alternative to glued-on bails is to fold the top of the glass pendant to create the channel for your cord or chain. These "fold-over" pendants can be both unique and elegant - and you never have to worry about a glue failure sending your glass crashing to the ground.

Here are some examples of fold-over pendants:


Finished Pendants.

 

This technique is accomplished without special tools and it does not require you to manipulate hot glass.

If it sounds difficult don't worry - it is exceptionally easy once you know how.

Are you ready to learn how to make fold-over pendants? Just click the link to step 1 below.

 

Awesome! I saw these at Helios...

I saw these at Helios and wondered how they were made!  Thanks for a great tutorial...very easy to understand!

Betsi - Avondale, AZ These

Betsi - Avondale, AZ

These look like such fun ... I can't wait to get started on making some. Thanks for sharing!

peggy chmiel

peggy chmiel

Comment viewing options

Select your preferred way to display the comments and click "Save settings" to activate your changes.