    Hello, I am fairly new to glass fusing and tonight tried to make circles.  I cut 1″ square to make circles which I would then make into flowers.  I thought when fired at full fuse (1500 degrees) they would end up as circles.  When finished cooling they were still square with rounded sides.  What did I do wrong?

    #13683

    wordana
    Participant

    Make sure to offset the top one a quarter turn to the bottom. You will need to fused fairly hot/long to get them to round out.

    Dana W.

    Fused Glass Designs

    dba Jester’s Baubles