    Hi all

    I really appreciate all the wisdom shared on this forum. I just bought a couple small ceramic bisque trays to use as slump molds. They are about 7 inches square. They have been fired to bisque. Should I fire them to their complete temperature? Or should I use them as bisque? If I fire them hotter will they last longer?

    Thanks for all help and info!!

    Liz

    #13665

    wordana
    Participant

    They will be fine to use if bisque-fired.

     